FREE shipping to on qualifying orders when you spend or more, processed by Ossila BV. All prices ex. VAT. Qualifying orders ship free worldwide! Fast, secure, and backed by the Ossila guarantee. It looks like you are visiting from , click to shop in or change country. Orders to the EU are processed by our EU subsidiary.

It looks like you are using an unsupported browser. You can still place orders by emailing us on info@ossila.com, but you may experience issues browsing our website. Please consider upgrading to a modern browser for better security and an improved browsing experience.

Aligned Multi-Walled Carbon Nanotubes

CAS Number 308068-56-6

Anode Materials, Battery Materials, Carbon Nanotubes (CNTs), Low Dimensional Materials, Materials


Product Code M2438L1-500mg
Price £60 ex. VAT

High Purity Aligned Multi-Walled CNTs

Improve mechanical and electrical properties of materials


Overview | Product Information | Related Products


Aligned multi-walled carbon nanotubes (MWCNTs), CAS number 308068-56-6, are arrayed in the same direction parallel to the bundle axis. Similar to other carbon nanotubes, aligned MWCNTs are widely used as reinforcing material to achieve high stiffness in polymer composites. Polymer composites incorporated with align multi-walled carbon nanotubes surpass those with ordinary MWCNTs (effective modulus of 6.4 GPa) in stiffness, exhibiting an effective modulus of 13.2 GPa.

Aligned multi-walled carbon nanotubes also enhance the electrical properties of polymer composites. An epoxy composite containing 0.01 wt% aligned multi-walled carbon nanotubes as conductive filler demonstrates a bulk conductivity of 10-3 S/m, transitioning from being purely dielectric. Additionally, the electrical conductivity of the polymer composites exhibits anisotropy. When measured parallel to the alignment of carbon nanotubes, the conductivity is nearly three orders of magnitude higher than when measured perpendicular to it.

Bundle axis aligned MWCNTs

Bundle axis aligned MWCNTs

Improving mechanical and electrical properties

Surpassing ordinary MWCNTs in stiffness

Surpassing ordinary MWCNTs in stiffness

Achieving an effective modulus of 13.2 Gpa

Worldwide shipping

Worldwide shipping

Quick and reliable shipping

High purity

High purity

>96% High purity

General Information


CAS Number 308068-56-6
Chemical Formula CxHy
Full Name Aligned multi-walled carbon nanotubes
Recommended Dispersants DI Water, DMF, THF, Ethanol, Acetone
Synonyms AMWCNT, A-MWCNT, Aligned multi walled carbon nanotubes
Classification or Family 1D materials, Carbon nanomaterials, Nanomaterials, Polycyclic aromatic hydrocarbons, Thin film electronics, Polymer composites

Aligned Multi-Walled Carbon Nanotubes


Product Code M2438L1 M2438L2
Purity >96% >96%
Outside Diameter 8 – 18 nm 8 – 18 nm
Inside Diameter 6 nm 5 – 10 nm
Length 9 – 14 μm 25 – 95 μm
Appearance Black powder Black powder
True Density 2.2 g/cm3 2.2 g/cm3
Specific Surface Area 30 – 300 m2/g 170 m2/g
Ash Content 2 wt% 2 wt%
Thermal Conductivity 2100 W/m·K N/A
Electrical Conductivity N/A 1300 S/cm
Manufacturing Method Chemical vapour deposition Chemical vapour deposition

MSDS Documentation


Aligned Multi-Walled Carbon NanotubesAligned Multi-Walled Carbon Nanotubes MSDS Sheet

Pricing


Product Code Product Details Quantity Price
M2438L1 9 – 14 μm length 500 mg £60
M2438L1 9 – 14 μm length 1 g £95
M2438L1 9 – 14 μm length 2 g £155
M2438L1 9 – 14 μm length 5 g £310
M2438L2 25 – 95 μm length 500 mg £60
M2438L2 25 – 95 μm length 1 g £95
M2438L2 25 – 95 μm length 2 g £155
M2438L2 25 – 95 μm length 5 g £350

References


  1. Investigation into the toughening mechanism of epoxy reinforced with multi-wall carbon nanotubes, X. Li et al., e-Polymers, 15 (5), 335–343 (2015); DOI: 10.1515/epoly-2015-0143.
  2. Anisotropic electrical conductivity of polymer composites with aligned carbon nanotubes, S. Gong et al., Polymer, 56, 498–506 (2015); DOI: 10.1016/j.polymer.2014.11.038.
  3. Formation of percolating networks in multi-wall carbon-nanotube–epoxy composites, C. Martin et al., Compos. Sci. Technol., 64, 2309–2316 (2004); DOI: 10.1016/j.compscitech.2004.01.025.

We stock a wide range of materials available to purchase online. Please contact us if you cannot find what you are looking for.

Return to the top