Ni-MWCNTs (Nickel Coated Multi-walled Carbon Nanotubes)
CAS Number 308068-56-6 / 7440-02-0
Anode Materials, Carbon Nanotubes (CNTs), Low Dimensional Materials, Materials
High purity high nickel content coated multi-walled carbon nanotubes of different sizes
For applications in hydrogen storage, catalysts, solar cells, and biosensors
Ni-MWCNTs (nickel coated multi-walled carbon nanotubes) is ferromagnetic nickel coated on one dimensional multi-walled carbon nanotubes framework, showing good magnetic properties.
With excellent electrical conductivity, remarkable chemical stability, and high number of active sites, Ni-MWCNTs exhibit excellent oxygen evolution reaction (OER) catalytic performance. Nickel impregnated multi-walled carbon nanotubes has also been used in dye sensitized solar cells (DSSCs) to replace the platinum counter electrode material, exhibiting a higher power-conversion-efficiency (PCE) of 9.72% while compared to that of Pt-based DSSC (8.85%).
Highly Conductive
Excellent electrical conductivity
High Purity
≥99% Ni-MWCNTs Purity
Low Cost
Low Cost Ni-MWCNTs
Various Applications
Applications in hydrogen storage, catalysts, solar cells, and biosensors
Other potential applications of Nickel-coated MWCNTs include electric-electronics, chemical energy, display technology, hydrogen storage, catalysts, biosensors, transistors, and drug delivery.
Literature
-
Ni-doped carbon nanotubes fabricated by pulsed laser ablation in liquid as efficient electrocatalysts for oxygen evolution reaction, S. Kang et al., Appl. Surf. Sci., 547, 149197 (2021); DOI: 10.1016/j.apsusc.2021.149197.
-
Nickel impregnated multi-walled carbon nanotubes (Ni/MWCNT) as active catalyst materials for efficient and platinum-free dye-sensitized solar cells (DSSCs), U. Mehmood et al., Sustainable Energy Fuels, 3, 3473-3480 (2019); DOI: 10.1039/C9SE00583H.
-
Synergetic Effect of Ni@MWCNTs and Hybrid MWCNTs on Electromagnetic Interference Shielding Performances of Polyurethane–Matrix Composite Foams, G. Sang et al., Ind. Eng. Chem. Res., 59 (34), 15233–15241 (2020); DOI: 10.1021/acs.iecr.0c01766.
-
The synthesized nickel-doped multi-walled carbon nanotubes for hydrogen storage under moderate pressures, S. Kaskun et al., Int. J. Hydrog. Energy, 43 (23), 10773-10778 (2018); DOI:10.1016/j.ijhydene.2018.01.084.
-
Nickel Nanoparticles on Carbon Nanotubes: Synthesis, Characterization and Hydrogen Storage, M. Figueroa-Torres, et al., J. New Mat. Electrochem. Systems,13 (3), 277-282 (2010); DOI: 10.14447/jnmes.v13i3.170.
- Ferromagnetic behaviour of nickel contacted multiwalled carbon nanotubes, E. Titus et al., J. Nanosci. Nanotechnol., 10 (4), 2606-2610 (2010); DOI: 10.1166/jnn.2010.1452.
Technical Data
CAS Number |
308068-56-6 (Carbon nanotubes) 7440-02-0 (Nickel) |
---|---|
Chemical Formula | Ni-C |
Synonyms | Nickel Doped Multi-Walled Carbon Nanotubes, Ni-MWCNT |
Classification / Family | 1D materials, Carbon nanomaterials, Nanomaterials, Polycyclic aromatic hydrocarbons, thin-film electronics |
Multi-Walled Carbon Nanotube Powders
Product code | M2412A1 | M2412B1 | M2412C1 |
---|---|---|---|
Inner Diameter | 2 – 5 nm | 5 – 10 nm | 5 – 15 nm |
Outer Diameter | 4 – 16 nm | 18 – 28 nm | 28 – 48 nm |
Nickel Content | 60% | 60% | 60% |
CNTs Content | 38% | 38% | 38% |
Length | 55 μm | 15 – 35 μm | 15 – 35 μm |
Tap Density | 0.3 g/cm3 | 0.3 g/cm3 | 0.3 g/cm3 |
Synthetic Method | CVD | CVD | CVD |
Color | Black | Black | Black |
Purity | >99% | >99% | >99% |
*For larger orders, please contact us to discuss prices.