Aluminum Oxide (Al2O3) Powder
CAS Number 1344-28-1
2D Materials, Inorganic Electronic Materials, Low Dimensional Materials, Materials, Metal OxidesHydrophilic γ-Al2O3 nanoparticles with ~ 18 nm ave. particle size, >99.5% purity
High purity gamma-phase aluminum oxide powders for application as catalysts, in water treatment, organic electronics and more.
Technical Data | MSDS | Literature and Reviews
Aluminum oxide (Al2O3, CAS number 1344-28-1), known as alumina, is one of the most frequent metal oxides used in industry due to its abundance in nature and low-cost production. Alpha (α), Beta (β) and gamma (ƴ) are the most well-known phase modifications of aluminum oxide.
γ-Al2O3 is used as a carrier of catalysts and a desiccant in processes of chemical and petrochemical production owing to its high surface area with open porosity and relatively stable over the temperature range of interest for most catalytic reactions. Aluminum oxide nanoparticles can also serve as additives to concrete mixtures, cosmetics, and textile industries. Aluminum oxide nanoparticles have also been used as antibacterial agent for biomedical purposes. Owing to its electrical resistance, aluminum oxide scaffold is beneficial for suppressing charge recombination, preventing moisture penetration, and increasing the thickness of light absorber layer in perovskite solar cells.
Alumina nanoparticles, mainly in α-and γ-forms, have been widely applied in adsorption-based applications because of their interesting properties such as high specific surface area (SSA), mechanical and thermal stability, inertness to most acids and alkalis, good electrical and chemical resistance in both oxidizing and reducing atmospheres up to 1000 °C, electrical insulation, high melting points, as well as being non-toxic and low-cost.
High purity
>99.5% purity
Worldwide shipping
Quick and reliable shipping
High SSA
~ 18 nm Particle size 140 m2/g SSA
Mechanical & Thermal stability
Stable over a wide temperature range
Technical Data
CAS Number | 1344-28-1 |
Chemical Formula | Al2O3 |
Molecular Weight | 101.96 g/mol |
Chemical Name | Aluminum oxide |
Synonyms | Alumina, Aluminum oxide |
Classification / Family | 2D semiconducting materials, nanomaterials, Solid lighting, metal oxides |
Colour | White powder |
Aluminum oxide (Al2O3) Powders
Product Code | M2400A1 |
Average Particle Size (APS) | ~ 18 nm |
Specific Surface Area (SSA) | 140 m2/g |
Specific Heat Capacity | 890 J/kg K |
True Density | 3.9 g/cm3 |
Melting Point | 2040 °C (lit.) |
Purity | > 99.5% |
Pricing Table
Product Code | Weight | Price |
M2400A1 | 50 g | £105 |
M2400A1 | 100 g | £165 |
M2400A1 | 250 g | £330 |
M2400A1 | 500 g | £520 |
*For larger orders please contact us to discuss prices
MSDS Documents
Aluminum Oxide Powders MSDS Sheet
Literatures
-
Preparation of γ-Al2O3 nanoparticles using modified sol-gel method and its use for the adsorption of lead and cadmium ions, J. Alloys Compd., S. Tabesh et al., 730, 441-449 (2018); DOI: 10.1016/j.jallcom.2017.09.246.
-
Cr3+ doped Al2O3 nanoparticles: Effect of Cr3+ content in intensifying red emission, P. Lewis et al., Curr. Appl. Phys., 32, 71-77 (2021); DOI: 10.1016/j.cap.2021.10.003.
- A novel foam formulation by Al2O3/SiO2 nanoparticles for EOR applications: A mechanistic study, H. Rezvani et al., J. Mol. Liq., 304, 112730 (2020); DOI: 10.1016/j.molliq.2020.112730.