FREE shipping to the United States on qualifying orders when you spend $300 or more. All prices ex. VAT. Enjoy hassle-free delivery, fulfilled by our EU subsidiary. Backed by our 50 State Delivery Guarantee. Regional distributors also available.

It looks like you are using an unsupported browser. You can still place orders by emailing us on info@ossila.com, but you may experience issues browsing our website. Please consider upgrading to a modern browser for better security and an improved browsing experience.

ITO Glass Substrates (Unpatterned)

Spectroscopy Equipment, Substrates and Fabrication

Product Code S111
In stock for priority dispatch
Price $169 ex. VAT

A Range of Unpatterned ITO Glass Substrates

Essential in a wide range of research applications


Transmittance | Characterization | Related Products | Resources and Support


Glass substrates coated with a 100 nm layer of indium tin oxide (ITO). Useful for a variety of experimental techniques including microscopy (STM, conductive AFM), spectroscopy, and electropolymerization.

Specifications


Substrate Sizes 20 mm x 15 mm
25 mm x 25 mm
25 mm x 75 mm (microscope slide)
Thickness 1.1 mm
Glass Type Polished soda lime, float glass
Substrate Coating Fully oxidized ITO
ITO Thickness 100 nm
ITO Quoted Resistance 20 Ω.□-1
ITO Measured Resistance* 14 - 16 Ω.□-1
Glass Roughness 1 nm RMS (by AFM)
ITO Roughness 1.8 nm RMS (by AFM)

* Resistances measured using the Ossila Four-Point Probe System.

ITO glass substrates

Please note: We does not offer custom substrate sizes. If you have a product suggestion, please contact us via our feedback page.

Transmittance of ITO Substrates

ITO Transmittance

Characterization

AFM scan of ITO substrate
10 µm x 10 µm AFM scan with Z-scale of ±5 nm
AFM of glass surface of ITO substrates
AFM of glass surface (1 µm x 1 µm x 3.5 nm)

The 20x15mm PV/OLED System

The 25x25mm PV/OLED System

The 75x25mm PV/OLED System

Resources and Support


OLED Fabrication GuideOLED Fabrication Guide

Fabricating OLED devices using Ossila’s pre-patterned ITO substrates is designed to be quick and easy. We've included every detail that we can in this manual so that you can produce efficient devices with as little effort as possible.

Read more...
OPV Fabrication GuideOPV Fabrication Guide

Within this guide, you’ll find comprehensive explanations for each step, along with additional tips and insights we’ve gathered to help you achieve the best possible results.

Read more...
Return to the top