FREE shipping to on qualifying orders when you spend or more, processed by Ossila BV. All prices ex. VAT. Qualifying orders ship free worldwide! Fast, secure, and backed by the Ossila guarantee. It looks like you are visiting from , click to shop in or change country. Orders to the EU are processed by our EU office.

It looks like you are using an unsupported browser. You can still place orders by emailing us on info@ossila.com, but you may experience issues browsing our website. Please consider upgrading to a modern browser for better security and an improved browsing experience.

Hexagonal Boron Nitride (h-BN) Crystals

CAS Number 10043-11-5

2D Materials, Hexagonal Boron Nitride, Low Dimensional Materials, Materials


Product Code M2133A1-5
Price $806 ex. VAT

Low price, high purity 2D hexagonal boron nitride (h-BN) crystals

Suitable for the creation of single or few-layer sheets via mechanical or liquid exfoliation


Product Information | MSDS | Literature and Reviews


Hexagonal boron nitride (h-BN) (CAS number 10043-11-5) has a honeycomb structure based on sp2 covalent bonds similar to graphene. Due to the similarity it is also known as “white graphene”. Unlike graphene, h-BN exhibits a wide band gap due to the difference in electronegativities of boron and nitrogen.

High Purity Hexagonal Boron Nitride

High Purity

High purity ≥99.99% Hexagonal Boron Nitride Crystal

Worldwide shipping for 10043-11-5

Worldwide Shipping

Quick and reliable shipping

Low price Hexagonal Boron Nitride (h-BN)

Low Price

Low price Hexagonal Boron Nitride (h-BN)

10043-11-5 Film & Crystals

Film & Crystals

Available in Film and crystal forms

h-BN is normally considered an insulator, and is used as a sub-layer material for any other 2D material in electronic devices. However, it has exotic opto-electronic properties (e.g. wide bandgap and low dielectric constant) along with mechanical robustness, high thermal conductivity and chemical inertness. It was later confirmed to have an indirect bandgap (at 5.955 eV), and thus is also considered a semiconductor.

2D h-BN has no absorption in the visible range, but has absorption in the ultraviolet region with good photoluminescence.

h-BN is widely used as a dielectric substrate in electronic and optical devices for graphene and other 2D-layered semiconductors (e.g. transition metal dichalcogenides TMDs).

Hexagonal boron nitride (h-BN) crystals are most commonly used as sources from which single or few-layer sheets can be obtained via either mechanical or liquid exfoliation.

h-BN has been used as a protective membrane in devices such as deep ultraviolet and quantum photonic emitters, where it provides strong oxidation resistance. It has also been utilised as a tunnelling barrier in field-effect tunnelling transistors.

Technical Data


CAS Number ‎10043-11-5
Full Name Hexagonal boron nitride
Chemical Formula BN
Molecular Weight 24.82 g/mol
Bandgap Indirect bandgap at 5.955 eV
Purity ≥99.99%
Preparation Synthetic - Chemical Vapour Transport (CVT)
Structure Hexagonal (2H)
Electronic Properties 2D Materials - insulator/semiconductor
Melting Point ‎‎2,973 °C (sublimates)
Colour Colourless
Synonyms White graphene, hexagonal BN, h-BN
Classification / Family 2D materials, Organic electronics, Materials science

Pricing Table


Product Code Form Package/Substrates* Price
M2133A1 Crystals Pack of 5 Crystals £520
M2133C1 Crystals Pack of 10 Crystals £900

*typical representative size, areas/dimensions may vary

**item with a lead time of 4 - 6 weeks, please contact for more information

Shipping is free for qualifying orders.

MSDS Documents


Hexagonal boron nitride Crystals MSDSHexagonal boron nitride Crystals MSDS

Literature and Reviews


  • Hexagonal boron nitride is an indirect bandgap semiconductor, G. Cassabois et al., Nat. Photon., 10, 262–266 (2016);DOI: 10.1038/NPHOTON.2015.277.
  • Graphene, hexagonal boron nitride, and their heterostructures: properties and applications, J. Wang et al., RSC Adv., 7, 16801 (2017); DOI: 10.1039/c7ra00260b.
  • Two dimensional hexagonal boron nitride (2D-h-BN): synthesis, properties and applications, K. Zhang et al., J. Mater. Chem. C, 5, 11992 (2017); DOI: 10.1039/c7tc04300g.


We stock a wide range of 2D materials available to purchase online. Please contact us if you cannot find what you are looking for.

Return to the top