Black Phosphorus Crystal
CAS Number 7723-14-0
2D Materials, Anode Materials, Battery Materials, Black Phosphorus, Low Dimensional Materials, Materials
Please choose the appropriate MSDS from the list below. Links will open in a new window. If your browser does not support PDFs, you will be prompted to download the file instead.
Low Price, High Purity Black Phosphorus Crystals
Available by weight or size for a wide range of applications
Overview | Product Information | MSDS | Related Products
Black phosphorus crystals (CAS number 7723-14-0) can be used to produce single or few-layer phosphorene sheets via mechanical or liquid exfoliation.
Superior to transition metal dichalcogenides, the bandgap of black phosphorus can be tuned with the number of layers but remains direct regardless of the film thickness. The sensitivity of black phosphorus ultrathin structures to the incident light opens the door for ultra-fast photodetectors from ultra-violet to near infrared region of the electromagnetic spectrum.
High Purity
High purity ≥99.995% black phosphorus crystals
Worldwide Shipping
Quick and reliable shipping
Low Cost
Low cost black phosphorus
Versatile
From gas sensors to next generation batteries
Black Phosphorus Small Crystal
Black phosphorus small crystals, available by weight with a metal-like lustre look and in high purity, contain various sizes of black phosphorus crystals or lumps. Black phosphorus small crystals are good for physical and chemical exfoliation and intercalation. This makes black phosphorus an ideal candidate for high-capacity rechargeable batteries, tuneable electronic devices, and superconductors.
Black Phosphorus Bulk Crystal
Available as bulk crystal in different sizes and in high purity, black phosphorus crystal is ideal for mechanical exfoliation to obtain multilayer to single layer two dimensional nanosheets or nanoparticles in application of transistors, optoelectronics, sensors, batteries and catalysis.
Technical Data
CAS Number | 7723-14-0 |
---|---|
Chemical Formula | P |
Molecular Weight | 30.97 g/mol |
Bandgap | 0.3 eV ~ 1.5 eV |
Synthesis | Synthetic, by chemical vapour transport |
Structure | Orthorhombic C |
Electronic Properties | 2D semiconductor |
Melting Point | 416 °C |
Colour | Black |
Form | Individual crystals |
Purity | ≥99.995% |
Pricing
Batch | Quantity | Price |
---|---|---|
M2106B1 | 250 mg | £480 |
M2106B1 | 500 mg | £850 |
M2106B1 | 1 g | £1,300 |
M2106A10 | Small (≥10 mm2) | £480 |
M2106A25 | Medium (≥25 mm2) | £700 |
MSDS Documentation
Black phosphorus small crystal
Related Products
We stock a wide range of low dimensional materials available to purchase online. Please contact us if you cannot find what you are looking for.