ITO Glass Substrates, 75 x 25 mm, PV and OLED
Materials, Solar Cell Prototyping Platform, Substrates and Fabrication
25 X 75 mm ITO patterned glass substrate, available with either modules or pixelated design. Perfect for use in OPV and OLED research.
The Pixelated Substrate System and Mini-Module Substrate System are designed to enable affordable scale-up. Alongside the Scale-Up Substrate Evaporation Masks, the substrates allow for larger devices and investigation of large-scale manufacturing techniques.
Datasheet
Size | 25 mm x 75 mm |
---|---|
Thickness | 1.1 mm |
Glass type | Polished soda lime, float glass |
Substrate coating | Fully oxidised ITO |
ITO thickness | 100 nm |
ITO resistance | 20 Ω/square |
Glass roughness | Less than 1 nm RMS (by AFM) |
ITO roughness | 1.8 nm RMS (by AFM) |