It looks like you are using an unsupported browser. You can still place orders by emailing us on info@ossila.com, but you may experience issues browsing our website. Please consider upgrading to a modern browser for better security and an improved browsing experience.

ITIC

CAS Number 1664293-06-4

Materials, Non-Fullerene Acceptors

Product Code M1101-100mg
Price $234

ITIC, acceptor molecule for non-fullerene organic solar cells

Low price, high purity (≥98%), ITIC available in sensible quantities


Specifications | MSDS | Literature and Reviews | Related Products


ITIC (CAS number 1664293-06-4) represents the start of a new generation of non-fullerene acceptors for organic photovoltaics (OPVs). The energy levels of ITIC allow for good alignment with low band-gap polymers, resulting in enhanced charge separation efficiency and reduced energy loss. ITIC molecules also have strong and broad absorption characteristics, from the visible region of the electromagnetic spectrum to the near infrared, peaking at 700 nm. This gives it the potential to increase the total absorption of an OPV device and enable improved power conversion efficiencies (PCEs). ITIC has also proved to have excellent thermal stability, with devices showing no losses after being held at 100 °C for 250 hours.

High efficient non-flullerene acceptor

High efficiency non-fullerene acceptor

with highly conjugated core

Enhances charge separation efficiency for low bandgap polymers

Enhances charge separation efficiency

with tailored energy level for low bandgap polymers

Worldwide shipping for 1664293-06-4

Worldwide shipping

Quick and reliable shipping

High purity

High purity

>98% High purity

These properties have resulted in ITIC becoming the first small molecule electron acceptor to outperform the most efficient fullerene acceptor, PC70BM, in an OPV device when fabricated in a controlled environment, such as a glove box. When used in conjunction with PBDB-T (PCE12) in an inverted-architecture device, ITIC enabled a power conversion efficiency of over 11% to be reached. By comparison, when PC70BM was used as the electron acceptor, a PCE of less than 8% was achieved.

ITIC from Ossila was used in the high-impact paper (IF 29.37)

ITIC from Ossila was used in the high-impact paper (IF 29.37), Triplet-Charge Annihilation in a Small Molecule Donor: Acceptor Blend as a Major Loss Mechanism in Organic Photovoltaics, J. Marin-Beloqui et al., Adv. Energy Mater., 2100539 (2021); DOI: 10.1002/aenm.202100539.

Most quantities are available for priority dispatch (lead times may apply for large quantities) and qualifying orders ship free as part of the Ossila Guarantee. Please contact us if you have any questions.

General Information


CAS Number 1664293-06-4
Chemical Formula C94H82N4O2S4
Purity ≥98.0% (1H NMR)
Full Name 3,9-bis(2-methylene-(3-(1,1-dicyanomethylene)-indanone))-5,5,11,11-tetrakis(4-hexylphenyl)-dithieno[2,3-d:2’,3’-d’]-s-indaceno[1,2-b:5,6-b’]dithiophene
Molecular Weight 1427.94 g/mol
HOMO / LUMO HOMO = -5.48 eV, LUMO = -3.83 eV [1]
Synonyms ITIC
Classification / Family Non-fullerene acceptors (NFAs), organic semiconducting materials, low band gap small molecule, small molecular acceptors (SMAs), organic photovoltaics, polymer solar cells, NF-PSCs, n-type

Chemical Structure


Chemical structure of ITIC (annotated)
The chemical structure of ITIC features (1) electron withdrawing substituents, (2) a central electron donating fused ring system, and (3) rigid side chains

Pricing


Batch Quantity Price
M1101 100 mg £180
M1101 250 mg £355
M1101 500 mg £570
M1101 1 g £915

MSDS Documentation


ITIC MSDSITIC MSDS Sheet


The ITIC family of NFAs includes ITIC and several derivatives, some of which offer higher power conversion efficiencies than ITIC itself. We stock a selection of high-purity ITIC derivatives for use in organic and polymer solar cells. Substituents such as fluorine and chlorine, which are electronegative, affect the HOMO and LUMO energy levels of ITIC-based acceptor molecules. In contrast, methyl groups can improve solubility, enhancing processability.

Literature and Reviews


  1. Non-Fullerene Polymer Solar Cells Based on Alkylthio and Fluorine Substituted 2D-Conjugated Polymers Reach 9.5% Efficiency, H. Bin et al., J. Am. Chem. Soc.,138 (2016), 4657−4664; DOI: 10.1021/jacs.6b01744.
  2. Fullerene-Free Polymer Solar Cells with over 11% Efficiency and Excellent Thermal Stability, W. Zhao et al., Adv. Mater., 28, 4734–4739 (2016); DOI: 10.1002/adma.201600281.
  3. An Electron Acceptor Challenging Fullerenes for Efficient Polymer Solar Cells, Y. Lin et al., Adv. Mater., 27, 1170–1174 (2015); DOI: 10.1002/adma.201404317.

Related Products


Non-Fullerene Acceptors Collection

Non-Fullerene Acceptors

Non-Fullerene Acceptors

Non-fullerene acceptors (NFAs) are a promising alternative to fullerene-based electron acceptors.

Semiconducting Polymers Collection

Semiconducting Polymers

Semiconducting Polymers

Semiconducting polymers for bulk heterojunction, OPV, OLED, OFET and perovskite interfaces and solar cell research.

Organic Conductors Collection

Organic Conductors

Organic Conductors

Organic conductors are an environmentally friendly alternative to traditional inorganic conductors.

Return to the top