FREE shipping on qualifying orders when you spend or more. All prices ex. VAT. Enjoy hassle-free delivery, fulfilled by our EU subsidiary. Backed by our 50 State Delivery Guarantee. Regional distributors also available. Sorry, we are unable to accept orders from or ship to .

It looks like you are using an unsupported browser. You can still place orders by emailing us on info@ossila.com, but you may experience issues browsing our website. Please consider upgrading to a modern browser for better security and an improved browsing experience.


Product Code M2260A1-100mg
Price $299 ex. VAT

PTO2, high quality polymer donor

Simple structure with great device performance efficiencies


Specifications | MSDS | Literature and Reviews


PTO2 is an alternating wide band-gap copolymer with electron-donating benzodithiophene (BDT) and electron-withdrawing thiophene carboxylate ester as the main backbone units. PTO2 enjoys good solubility in non-halogenated solvents, i.e. xylenes and THF.

With an efficient charge generation at a low driving force, an efficiency of 14.7% was achieved in a single-junction OPV by using polymer donor PTO2 and a non fullerene acceptor IT-4F.

PTO2 is considered as good replacement for PBDB-T-2F (PM6) or PTB7-Th for it similar but simpler structure, while maintaining great device performance efficiencies at lower costs.

Wide bandgap copolymer

Wide bandgap copolymer

For high efficient OPV applications

Luminosyn™

Luminosyn™

High purity, batch-specific GPC data, available larger batch orders and higher molecular weight

Worldwide shipping for PTO2

Worldwide shipping

Quick and reliable shipping

Green energy material

Green energy materials

Processable in non-halogenated solvents

PClTO2, a chlorine version of PTO2, is also available to our customers. Please refer to our collection of green energy materials for non-halogenated solvents processing choice of non-fullerene acceptors (NFAs).

Luminosyn™ PTO2


Luminosyn™ PTO2 is now available.

High purity

PBTO2 is purified by Soxhlet extraction with methanol, hexane and chlorobenzene under an argon atmosphere

Batch-specific GPC data

Batch specific GPC data is always available for your thesis or publication

Large-quantity orders

Plan your experiments with confidence with polymers from the same batch

General Information


Full name Poly[(2,6-(4,8-bis(5-(2-ethylhexyl-3-fluoro)thiophen-2-yl)-benzo[1,2-b:4,5-b’]dithiophene))-alt-(2,2-ethyl-3(or4)-carboxylate-thiophene)]
Synonyms PE12, PFTO2
Chemical formula (C41H44F2O2S5)n
CAS number n.a.
HOMO / LUMO HOMO = -5.56 eV, LUMO = -3.67 eV [2]
Soluble in THF, o-xylene, chloroform, chlorobenzene and dichlorobenzene
Recommended Processing Solvents at 10mg/ml THF (8mg/ml), o-xylene (8mg/ml), chloroform
Classification / Family Organic semiconducting materials, Wide band-gap polymers, Organic Photovoltaics, Polymer solar cells, NF-PSCs, All-polymer solar cells (all-pscs), Green energy materials.

Batch Details


Batch Mw Mn PDI Stock Info
M2260A1 63,527 29,379 2.16 Low stock
M2260A2 120,565 55,455 2.17 In stock

Chemical Structure


chemical structure of green material pto2 and solubility in THF and o-xylenen
Chemical structure of PTO2 (PE12) and its solubility in THF and o-xylene.

Device Structure


Device structure: ITO/PEDOT:PSS (10 nm)/PTO2:ITIC-4F (1:1, 100 ± 5nm)/PFN-Br (5 nm)/Al (80 nm)

Thickness (nm) VOC (V) JSC (mA cm-2) FF (%) PCE (%)
100 0.91 21.5 75.0 14.7

MSDS Documentation


PTO2 MSDSPTO2 MSDS sheet

Literature and Reviews


  1. Achieving Over 15% Efficiency in Organic Photovoltaic Cells via Copolymer Design, Y. Cui et al., Adv. Mater., 31 (14), 1808356 (2019); DOI: 10.1002/adma.201808356.
  2. Wide bandgap polymer donors for high efficiency non-fullerene acceptor based organic solar cells, K. He et al., Mater. Adv., 2, 115 (2021); DOI: 10.1039/d0ma00790k.
  3. 14.7% Efficiency Organic Photovoltaic Cells Enabled by Active Materials with a Large Electrostatic Potential Difference, H. Yao et al., J. Am. Chem. Soc., 141, 19, 7743–7750 (2019); DOI: 10.1021/jacs.8b12937.
Return to the top