PFN-bromide, PFN-Br
CAS Number 889672-99-5
Cathode Interlayer Materials (CIMs), Interface Polymers, Materials, Organic Conductors, Perovskite Interface Materials, Perovskite Materials,PFN-Br, used to improve extraction efficiencies in organic electronic devices
High quality polymer available for fast, secure dispatch
Overview | Specifications | Pricing and Options | MSDS | Literature and Reviews
With hydrophobic backbone and hydrophilic side chains, PFN-Br (CAS number 889672-99-5) is a conjugated polymer electrolyte (CPE). It serves as an electron-interface layer material in organic electronic devices (including OFET, OLED, OPV and perovskite solar cells) to improve the interfacial properties such as extraction efficiency.
PFN-Br interfacial layer embedded in OPV devices gives overall enhanced open-circuit voltage, short-circuit current density and fill factor thus improved device performance. It is also believed that the device performance of polymer LEDs with bilayer cathodes (e.g. PFN-Br/Al), can be enhanced to levels comparable to (and even higher than) those obtained from using Ca or Ba cathodes due to its strong polar ionic pendant groups.
Cathode interlayer molecule
For high efficient OPV applications
Improve extraction efficiency
as a conjugated polyelectrolyte
Worldwide shipping
Quick and reliable shipping
Enhance device performance
strong polar ionic pendant groups
PFN-Br has been used in highly efficient OPV tandem structures with device efficiency over 17%.
General Information
Full name | Poly(9,9-bis(3’-(N,N-dimethyl)-N-ethylammoinium-propyl-2,7-fluorene)-alt-2,7-(9,9-dioctylfluorene))dibromide |
Synonyms |
|
Chemical formula | (C56H80N2Br2)n |
CAS number | 889672-99-5 |
Classification/Family | Conjugated polymers, Polymer electrolyte, Polyfluorenes, Electron interface layer materials, OLED, OPV, Perovskite materials |
Chemical Structure

Batch information
Batch | Mw | Mn | PDI | Stock info |
M2230A1 | 165 kDa | 57 kDa | 2.9 | Discontinued |
M2230A2 | 190 kDa | 61 kDa | 3.1 | Discontinued |
M2230A3 | 84 kDa | 40 kDa | 2.1 | Discontinued |
M2230A4 | 131 kDa | 42 kDa | 3.1 | In Stock |
Pricing
Batch | Quantity | Price |
M2230A | 100 mg | £280 |
M2230A | 250 mg | £560 |
M2230A | 500 mg | £950 |
MSDS Documentation
Literature and References
- Efficient Electron Injection from a Bilayer Cathode Consisting of Aluminum and Alcohol-/Water-Soluble Conjugated Polymers, H. Wu et al., Adv. Mater., 16, 1826–1830 (2004), DOI: 10.1002/adma.200400067.
- High-Performance Polymer Solar Cells Based on a Wide Bandgap Polymer Containing Pyrrolo[3,4- f]benzotriazole5,7-dione with a Power Conversion Efficiency of 8.63%, L. Lan et al., Adv. Sci., 3, 1600032 (2016); DOI: 10.1002/advs.201600032.
- Toward high performance inverted polymer solar cells, X. Gong et al., Polymer 53, 5437e5448 (2012); DOI: 10.1016/j.polymer.2012.09.023.