Lithium Nickel Cobalt Aluminum Oxide (NCA) Powder
CAS Number 193214-24-3
2D Materials, Battery Materials, Cathode Active Materials, Inorganic Electronic Materials, Low Dimensional Materials, Materials,Layered LiNi0.8Co0.15Al0.05O2 Powder, NCA Cathode Material
High voltage, good rate capability and cycling stability NCA cathode material for HEV and PHEV
Product Information | MSDS | Literature and Reviews | Related Products
Lithium nickel cobalt aluminum oxide (NCA) cathode material, CAS number 193214-24-3, is considered one of the most promising of the next generation cathode materials that provides higher capacity than LiCoO2, especially for HEV and PHEV due to its high energy density, high thermal stability, and low toxicity.
Faster Charging
Faster charging & High Voltage
High Thermal Stability
High thermal stability Battery Materials
Low Toxicity
Low toxicity Battery Materials
Worldwide Shipping
Quick and reliable shipping
It has been well known that carbon nanotubes, other metal or metal oxides modified lithium cathode materials can help to improve the battery capacity and durability. With a relatively larger ion radius, titanium ions could modify the oxygen lattice and change the local coordination environment of the layered lithium nickel cobalt aluminum oxide, resulting in decreased cation migration, better kinetic and thermodynamic properties, and improved structural stability. Ti-substituted NCA cathode exhibits impressive reversible capacity (198 mA h g-1 at 0.1 C) with considerable cycle stability under a cut-off voltage up to 4.7 V.
Product Information
CAS Number | 193214-24-3 |
---|---|
Chemical Formula | LiNi0.8Co0.15Al0.05O2 |
Molecular Weight | 183.54 g/mol |
Chemical Name | Lithium Nickel Cobalt Aluminum Oxide |
Synonyms | NCA, LNCA |
Classification / Family | 2D semiconducting materials, Battery materials, Metal oxides, Cathode materials |
Colour | Black to grey powder |
Technical Data
Product Code | M2404A1 |
---|---|
Li | 7.15% |
Al + Co + Ni | 58.70% |
Li2CO3 | 0.22% |
LiOH | 0.18% |
BET | 0.30 m2/g |
Tap Density | 2.68 m2/g |
Compact Density | 3.1 g/cm3 |
Particle Size | ~13 µm |
pH | 11.62 |
Pricing Table
Product Code | Weight | Price |
---|---|---|
M2404A1 | 10 g | £105 |
M2404A1 | 25 g | £210 |
M2404A1 | 50 g | £330 |
M2404A1 | 100 g | £400 |
*For larger orders please email us to discuss prices.
MSDS Documents
Lithium Nickel Cobalt Aluminum Oxide (LiNi0.8Co0.15Al0.05O2) Powder MSDS Sheet
Literature and Reviews
-
LiNi0.8Co0.15Al0.05O2 cathode modified by nitroxide radical for lithium-ion battery with high capacity, M. Li et al., Mater. Today Commun., 34, 105360 (2023); DOI: 10.1016/j.mtcomm.2023.105360.
-
Insight into thermal analysis kinetics of surface protected LiNi0.8Co0.15Al0.05O2 cathode for safe lithium-ion batteries, Energy Stor. Mater., 49, 409-420 (2022); DOI: 10.1016/j.ensm.2022.04.014.
-
Boosting Cell Performance of LiNi0.8Co0.15Al0.05O2 via Surface Structure Design, J. Zheng et al., Small, 15 (50), 1904854 (2019); DOI: 10.1002/smll.201904854.
Related Products
We stock a wide range of Battery Materials available to purchase online. Please contact us if you cannot find what you are looking for.