A metal oxide widely used in batteries

owing to its low cost, sustainability, and high theoretical capacity, MnO2


Overview | Product Information | Related Products


Manganese (IV) oxide (CAS number 1313-13-9) is tetravalent and predominantly used in the battery industry. It is used extensively in Zn-ion batteries, due to its low cost, high theoretical capacity and sustainability. Zn/MnO2 batteries exhibit high stability, an excellent gravimetric capacity of 450 mAh/g and a 90% capacity retention. They provide an energy density of 150 Wh/kg even under high temperature up of to 55°C.

Manganese oxide can also be used to dope spiro-OMeTAD, for early and rapid oxidation of spiro-OMeTAD precursor solution, mitigating the adverse effects of air oxidation. This MnO2-doped hole transport layer demonstrates improved morphology, conductivity and better aligned HOMO level with the perovskite active layer. As a result, the external quantum efficiency increases from 83% to 87.6%.

Manganese oxide

Metal oxide

widely used in batteries

Green energy material

Green energy material

low cost, good sustainability, and high capacity

Quick and reliable shipping

Worldwide shipping

Quick and reliable shipping

High purity

High Purity

99%

General Information


CAS Number 1313-13-9
Chemical Formula MnO2
Full Name Manganese dioxide
Molecular Weight 86.94 g/mol
Melting Point 535 °C (decompose)
Synonyms Manganese oxide, Dioxomanganese
Classification or Family Metal oxides, Battery materials, Perovskite solar cells

Product Details


Purity 99%
Particle Size ≤ 100 nm
Appearance Black powder

MSDS Documentation


Manganese (IV) Oxide MSDS SheetManganese (IV) Oxide MSDS Sheet

References


  • A key advance toward practical aqueous Zn/MnO2 batteries via better electrolyte design, I. Aguilar et al., Joule, 9, 101784 (2024); DOI: 10.1016/j.joule.2024.11.001.
  • Recent advances on challenges and strategies of manganese dioxide cathodes for aqueous zinc-ion batteries, Y. Xu et al., Energy Environ. Mater., 6, e12575 (2023); DOI: 10.1002/eem2.12575.
  • Low-cost manganese dioxide semi-solid electrode for flow batteries, T. Narayanan et al., Joule, 5, 2934–2954 (2021); DOI: 10.1016/j.joule.2021.07.010.


We stock a wide range of Metal Oxides available to purchase online. Please contact us if you cannot find what you are looking for.

Cathode Active Materials Collection

Cathode Active Materials

Cathode Active Materials

Explore the range of high-purity cathode materials including NMC and LCO.

Metal Oxide Collection

Metal Oxides

Metal Oxides

A range of metal oxides for application in batteries and much more.

Anode Active Materials Collection

Anode Active Materials

Anode Active Materials

Explore the range of anode active materials including graphite.

Return to the top