Hydroxylated single-walled carbon nanotubes (SWCNT-OH)

as functionalized SWCNTs applied in a wide range of applications including sensors, batteries, and polymer reinforcement


Overview | Product Information | Related Products


OH functionalized single-walled carbon nanotubes (SWCNT-OH) are hydroxylated SWCNTs with hydroxy groups attached to the surface of the nanotubes. Compared to pristine SWCNTs, SWCNT-OH has a propensity to trap electrons, leading to its applications in dye-sensitized solar cells, hydrogen evolution, and CO2 reduction. The standard rate constant of the heterogeneous electron transfer between Fe(CN)63−/4− and SWCNT-OH is 25.9 × 10−4 cm/s, which is four times higher than that of pristine SWCNTs.

The OH groups in SWCNT-OH enhance the dispersibility of the CNTs. The improved homogeneity of the composites promotes better mechanical properties and higher thermal stability. The hydroxy groups on the surface of the CNTs can form hydrogen bonds with other materials such as PEDOT:PSS. The intermolecular interaction extends the polymeric conformation of PEDOT, facilitating the electron conduction. This results in a greater power factor (PF) in thermoelectric devices, exhibiting an increased PF from 0.7 μW/m·K2 to 22 μW/m·K2.

High Purity Multi-Walled Carbon Nanotubes

High Purity

>92% OH functionalized SWCNTs

Worldwide shipping for 308068-56-6

Worldwide Shipping

Quick and reliable shipping

Reduced cost in synthesis with 308068-56-6

Low Cost

Reduced cost in synthesis

Applications of Multi-Walled Carbon Nanotubes

Versatile Applications

Improve mechanical or electrical properties

General Information


CAS Number 308068-56-6
Chemical Formula CxHyOz
Full Name Hydroxylated single-walled carbon nanotubes
Recommended Dispersants DI water, DMF, THF, ethanol, and acetone
Synonyms OH single-walled carbon nanotubes, Hydroxylated single-walled carbon nanotubes, Hydroxy single-walled carbon nanotubes, OH SWCNTs, SWCNT-OH, OH single-walled CNTs
Classification or Family 1D materials, Carbon nanomaterials, Nanomaterials, Polycyclic aromatic hydrocarbons, thin-film electronics
Appearance Black fibrous powder

Chemical Structure


OH functionalized single-walled carbon nanotubes, SWCNT-OH, CAS number 308068-56-6

Product Details


Product Code M2015L3 M2395B1
Diameter (nm) 2 1 – 2
Length (μm) 5 – 20 1 – 3
OH Content (wt%) 4 4
Specific surface Area (m2/g) 450 370
Purity (%) 95% > 92%

MSDS Documentation


OH functionalized single-walled carbon nanotubesOH functionalized single-walled carbon nanotubes MSDS sheet

References


  • Enhanced thermoelectric properties of PEDOT:PSS composites by functionalized single wall carbon nanotubes, M. Tonga et al., Int. J. Energy Res., 44, 9149–9156 (2020); DOI: 10.1002/er.5535.
  • The hydroxylated carbon nanotubes as the hole oxidation system in electrocatalysis, P Szroeder et al., Materials, 17, 3532 (2024); DOI: 10.3390/ma17143532.
  • Sulfur dioxide detection using composite of nickel benzene carboxylic (Ni3BTC2) and OH-functionalized single walled carbon nanotubes (OH-SWCNTs), N. Ingle et al., Front. Mater., 7, 93 (2020); DOI: 10.3389/fmats.2020.00093.