It looks like you are using an unsupported browser. You can still place orders by emailing us on info@ossila.com, but you may experience issues browsing our website. Please consider upgrading to a modern browser for better security and an improved browsing experience.


Product Code B4171-250mg
Price $65

Covalent Organic Frameworks (COFs) Bis(allyloxy)benzene Ligand

Substituted with hydrazide groups for the synthesis of COFs in the applications of batteries, sensors, catalysts, and optoelectronics


Overview | Product Information | MSDS | Related Products


2,5-Bis(allyloxy)terephthalohydrazide (CAS number 2227151-69-9) is a benzene building block substituted with two allyloxy groups and two hydrazides. The hydrazide groups in 2,5-bis(allyloxy)terephthalohydrazide react with aldehyde derivatives to form COFs with hydrazone linkages. The allyloxy groups allow the resulting COFs to be further functionalized with alkene such as poly(ethylene glycol) methyl ether methacrylate (PEGMA), via radical polymerization. The COF-PEGMA is applied as a solid-state electrolyte for lithium batteries, exhibiting high ionic conductivity of 5.3 × 10−5 S/cm and lithium ion transference number of 0.47.

The allyloxy pendant groups in COFs can function as Hg2+ acceptors. Additionally, the binding of Hg2+ quenches the fluorescence of the COFs. Thus, they are used for selective mercury ion detection in applications of water purification.

MOF and COF ligands

MOF and COF Ligands

bis(allyloxy)benzene ligand for cross-linked COF/MOF networks

Facile reactions

Facile Reactions

Hydrazide possesses excellent reactivity

High purity

High Purity

>97% pure

Worldwide shipping for 2227151-69-9

Worldwide Shipping

Quick and reliable shipping

General Information


CAS Number 2227151-69-9
Chemical Formula C14H18N4O4
Full Name 2,5-Bis(allyloxy)terephthalohydrazide
Molecular Weight 306.32 g/mol
Synonyms 2,5-Bis(prop-2-en-1-yloxy)benzene-1,4-dicarbohydrazide, 2,5-Diallyloxybenzene-1,4-dicarbohydrazide, BATH
Classification or Family Porous organic frameworks, COFs, Hydrazides, Allyls, Batteries, Electrolytes

Chemical Structure


2,5-Bis(allyloxy)terephthalohydrazide chemical structure, CAS 2227151-69-9
2,5-Bis(allyloxy)terephthalohydrazide chemical structure, CAS 2227151-69-9

Product Details


Purity > 97%
Melting Point N/A
Appearance Off-white fluffy powder

MSDS Documentation


2,5-Bis(allyloxy)terephthalohydrazide MSDS Sheet2,5-Bis(allyloxy)terephthalohydrazide MSDS Sheet

References


  • Application of synthesized 2,5-bis(allyloxy)terephthalohydrazide functionalized covalent organic framework material as a fluorescence probe for selective detection of mercury (II)Y. Yin et al., Mater. Today Commun., 27, 102440 (2021); DOI: 10.1016/j.mtcomm.2021.102440.
  • Covalent organic framework supported palladium catalysts, H. Salemi et al., J. Mater. Chem. A, 10, 20707 (2022); DOI: 10.1039/d2ta05234b.
  • Flexible solid-state electrolyte based on comb-like PEG-functionalized covalent organic frameworks for lithium metal batteries, X. Tan et al., Polym. Chem., 15, 454–464 (2024); DOI: 10.1039/D3PY01265D.


We stock a wide range of porous organic frameworks available to purchase online. Please contact us if you cannot find what you are looking for.

Return to the top